dc.description | The high temperature apparatus developed in the Department of Materials for the torsional creep testing of graphite at temperatures up to 3000 oC has been utilised to heat-treat tungsten-thoria alloys at temperatures up to 2500 oC. Modifications to the torsional loading system have enabled some of these heat-treatments to be carried out under an applied stress. | |
dc.language | en | |
dc.publisher | College of Aeronautics | |
dc.relation | CoA/M/Mat-56 | |
dc.relation | 56 | |
dc.title | Experimental techniques used in the high temperature heat-treatment of some tungsten-thoria alloys | |