Test report no. PLBO/17 crater wear of tips grade SIP, RD176, RD110 and RD184 machining EN9

Show simple item record

dc.creator College of Aeronautics, (Cranfield)
dc.date 2016-10-21T14:18:57Z
dc.date 2016-10-21T14:18:57Z
dc.date 1965-02
dc.date.accessioned 2022-05-09T10:03:02Z
dc.date.available 2022-05-09T10:03:02Z
dc.identifier http://dspace.lib.cranfield.ac.uk/handle/1826/10826
dc.identifier.uri https://reports.aerade.cranfield.ac.uk/handle/1826.2/4339
dc.description Tests were carried out with tools of grade S1P„ RD1841 RD110 and RD176 at 600 fpm cutting speed, 0.010 in/rev. feed and 0.10 in. depth of cut machining EN9 to determine their relative resistance to crater wear. The performance of the grades was in the ratio S1P-100, RD184-85„ RD110-56 and RD176-53, although with three out of the four corners tested the performance of RD184 matched that of S1P. During the tests RD184 was the only grade which had an edge radius and it is suggested that further tests should be carried out to determine whether this has any effect on cratering.
dc.language en
dc.publisher College of Aeronautics
dc.relation CoA/M/M&P-59
dc.relation 59
dc.title Test report no. PLBO/17 crater wear of tips grade SIP, RD176, RD110 and RD184 machining EN9
dc.type Report


Files in this item

Files Size Format View
COA_M_M+P_59_1965.pdf 375.1Kb application/pdf View/Open